SpecificationBrand : Gdrasuya10
BulletPoint1 : ▶Heat the acetylene flame on the workpiece to 300-400 degrees Celsius.
BulletPoint2 : ▶The distance between the nozzle and the workpiece surface is 120~150 mm. At the same time, the self-fluxing alloy powder can be evenly sprayed on the surface of the workpiece, and then melted by the flame to appear on the surface mirror surface, gradually moving the melting position, so that the alloy powder and the workpiece are polarized and dispersed. Forming an adhesive layer
BulletPoint3 : ▶Different alloy powders can be used to obtain different properties of wear-resistant and corrosion-resistant layers.
BulletPoint4 : ▶Due to the uneven particle size of the powder, or becoming wet, the powder valve switch is invalidated and blocked, and should be repaired in time. If it is used again, dry powder must be used.
BulletPoint5 : ▶Clean the spray gun regularly to avoid obstruction of the air tube hole. When cleaning the tube hole, pop up and clean the powder feeder.
ExternallyAssignedProductIdentifier1 : 0723509123260
ExternallyAssignedProductIdentifier2 : 723509123260
ItemName : Gdrasuya10 Welding Gun Spray Metal Powder Torch, Q-1/H Flame Welding Gun Metal Powder Spray Gas Welding Torche Oxygen Acetylene Flame Gun
ItemTypeKeyword : soldering-torches
Manufacturer : ZONGFOW
Material : Metal
PartNumber : BI-LMLZBY-1194-Z
ProductDescription :
Product specifications:
Model:Q-1/H
Nozzle Diameter: 3pcs (0.9 /1.1/1.3)
Power Velocity: 0.4-0.6/0.6-0.8/0.8-1.0
Length: 430mm
Gas type: O2, C2H2 (acetylene)
The package includes:
3 x Welding nozzle
1 x The connecting nuts
1 x Powder bucket seat
1 x Powder hopper
1 x Control powder feeder
1 x Powder pressing hand
1 x Oxygen joint
1 x The acetylene joint
Product description:
★ Heat the acetylene flame on the workpiece to 300-400 degrees Celsius.
★The distance between the nozzle and the workpiece surface is 120~150 mm. At the same time, the self-fluxing alloy powder can be evenly sprayed on the surface of the workpiece, and then melted by the flame to appear on the surface mirror surface, gradually moving the melting position, so that the alloy powder and the workpiece are polarized and dispersed. Forming an adhesive layer
★ Different alloy powders can be used to obtain different properties of wear-resistant and corrosion-resistant layers.
★ Due to the uneven particle size of the powder, or becoming wet, the powder valve switch is invalidated and blocked, and should be repaired in time. If it is used again, dry powder must be used.
★ Clean the spray gun regularly to avoid obstruction of the air tube hole. When cleaning the tube hole, pop up and clean the powder feeder.
ProductSiteLaunchDate : 2020-12-30T09:56:05.474Z
UnspscCode : 23271800