Specification Brand : Mai LELU BulletPoint1 : - Copper pipe, surface chrome plating treatment, not easy to age, long service life. BulletPoint2 : - The accessories in the product packaging are various and can be replaced. BulletPoint3 : - The components are finely crafted, divided into oxygen and gas interfaces, and are convenient to use. BulletPoint4 : 【Note】- Due to the uneven particle size of the powder, or becoming wet, the powder valve switch is invalidated and blocked, please repair it in time. When used again, must use dry powder; Clean the spray gun regularly to avoid obstruction of the air tube hole; when cleaning the tube hole, pop up and clean the powder feeder. BulletPoint5 : 【Package Includes】- 3x Welding Nozzle; 1x Connecting Nut; 1x Powder Bucket Seat; 1x Powder Hopper; 1x Control Powder Feeder; 1x Powder Pressing Hand; 1x Oxygen Joint; 1x Acetylene Joint Color : Silver ExternallyAssignedProductIdentifier1 : 0752692417443 ExternallyAssignedProductIdentifier2 : 752692417443 IncludedComponents : 1 x Set of Metal Powder Spray Welding Torch ItemName : Metal Powder Spray Welding Torch Oxygen Acetylene/Oxygen Propane Portable Flame Welding Gun QHT-7/h ItemPackageDimensions_Height : 4 centimeters ItemPackageDimensions_Length : 25.7 centimeters ItemPackageDimensions_Width : 12 centimeters ItemPackageQuantity : 1 ItemTypeKeyword : soldering-torches Manufacturer : Alff Material : Metal Material1 : Stainless Steel Material2 : Acrylonitrile Butadiene Styrene (ABS) Material3 : Copper MaximumTemperature : 752 degrees_fahrenheit ModelName : QHT-7/h metal powder spray welding torch ModelNumber : a275 NumberOfItems : 1 PartNumber : YOCXJBPUQ9R8U PowerSourceType : Gas ProductDescription : Working principle and application of QHT-7/h metal powder spray welding torch: - Use an oxyacetylene flame to heat the sprayed workpiece to about 300-400 degrees Celsius; - Then make the nozzle 120-150 millimeters away from the workpiece surface. Spray the self fusing alloy powder evenly on the workpiece surface; - After the flame melts until the mirror reflection appears on the workpiece surface, gradually move the melting position so that the alloy powder and the workpiece base metal are mutually deposited, diffusing each other to form a firm bonding layer.
* Using different kinds of alloy powder, can get the abrasion resistance, corrosion resistance and other different properties of strengthened layer.
Note: 1. Medium pressure type structure, it must be used in the medium pressure acetylene generator and an acetylene cylinder pipe, absolutely should not be used in low pressure acetylene generator and pipeline. 2. Spray gun, if no ignition, can not press powder valve switch, to avoid blockage. 3. Due to the powder 's particle size is not uniform, or become damp and other factors, make the powder valve switch failure, clogging, it shouold be repaired in time before be used again . 4. Attention --must use dry powder. 5. Regular cleaning spray gun, in order to avoid the gas tube holes are blocked. while cleaning pipe hole ,ejects out and clean up the control powder feeder. 6. Keep the gas pipeline drying, smooth to avoid damp effect of powder. 7. All the pipelines of spray welding torch are not contaminated oil, to prevent oxygen meet oil to have combustion and explosion. 8. Spray gun at the end of work, first close the acetylene valve, and then use the oxygen blowing internal pipeline, after liquidation shall be sprayed welding torch and hose hanging, prevent dust and impurity invasion of spray welding nozzle, to effect the normal use. 9. The use of spray welding torch, oxygen, acetylene pipeline must be equipped with a backfire preventing device.